Polayên kêm-alloy Manual elektrodê E8018-C2 Daneyên zeliqandinê
KOMPONETA KÎMYYA:
ALLOY(wt%) | C | Mn | Si | Ni | Cr | Mo | P | S |
GB / T RULES | 0.12 | 1.25 | 0.80 | 3.00-3.75 | - | - | 0.03 | 0.03 |
AWS RULES | 0.12 | 1.25 | 0.80 | 3.00-3.75 | - | - | 0.03 | 0.03 |
MÎNAK NIRX | 0.045 | 0.75 | 0.22 | 3.52 | 0.04 | 0.06 | 0.007 | 0.004 |
TAYBETÎ MÊKANÎK:
MAL | HÊZA BERHEMÊ (MPa) | XWEZAYÊ BERÊRÊKIRIN (MPa) | NIRXA IMAPACT J/℃ | DIRÊZ (%) | Tedawiya germê ° Cxh | |||||
GB / T RULES | 460 | 550 | 27/-75 | 17 | 605*1 | |||||
AWS RULES | 460 | 550 | 27/-75 | 19 | 605*1 | |||||
MÎNAK NIRX | 495 | 600 | 100/-75 | 26 | 605*1 |
PÊŞNÎŞAN PARAMETÊN WELDING:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELATRÎK (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |
Iron toza low hydrogen type elektrodê destê.
Ji ber lêzêdekirina toza hesin, karbidestiya helandinê bilindtir e, hişkiya bandorê ya metala şilkirî li -75℃.
Kevana stabîl, kêm rijandin, pêkhatina baş, rakirina slaqê hêsan, performansa X-Ray xweş e.
KOMPONETA KÎMYYA:
ALLOY(wt%) | C | Mn | Si | Ni | Cr | Mo | P | S |
GB / T RULES | 0.12 | 1.25 | 0.80 | 3.00-3.75 | - | - | 0.03 | 0.03 |
AWS RULES | 0.12 | 1.25 | 0.80 | 3.00-3.75 | - | - | 0.03 | 0.03 |
MÎNAK NIRX | 0.045 | 0.75 | 0.22 | 3.52 | 0.04 | 0.06 | 0.007 | 0.004 |
TAYBETÎ MÊKANÎK:
MAL | HÊZA BERHEMÊ (MPa) | XWEZAYÊ BERÊRÊKIRIN (MPa) | NIRXA IMAPACT J/℃ | DIRÊZ (%) | Tedawiya germê ° Cxh | |||||
GB / T RULES | 460 | 550 | 27/-75 | 17 | 605*1 | |||||
AWS RULES | 460 | 550 | 27/-75 | 19 | 605*1 | |||||
MÎNAK NIRX | 495 | 600 | 100/-75 | 26 | 605*1 |
PÊŞNÎŞAN PARAMETÊN WELDING:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELATRÎK (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||